The spin coater is located in the Durand Building [https://www.google.com/maps/place/Durand+Building,+496+Lomita+Mall,+Stanford,+CA+94305/@37.4268696,-122.1754608,17z/data=!3m1!4b1!4m5!3m4!1s0x808fbb2aa1a2e6c7:0x150c778bd3b558cf!8m2!3d37.4268696!4d-122.1732721 (address)] in room 150. This is the lab directly to the right of the first floor entrance. The spin coater is a model PWM32-PS-CB15 Spinner System developed by Headway Research, Inc.
+
[[File:spinner.jpg|200px|thumb|right|Image of the Durand Spin Coater.]]
 +
The spin coater is located in the Durand Building  
 +
[https://www.google.com/maps/place/Durand+Building,+496+Lomita+Mall,+Stanford,+CA+94305/@37.4268696,-122.1754608,17z/data=!3m1!4b1!4m5!3m4!1s0x808fbb2aa1a2e6c7:0x150c778bd3b558cf!8m2!3d37.4268696!4d-122.1732721 (address)] in room 150. This is the lab directly to the right of the first floor entrance. The spin coater is a model PWM32-PS-CB15 Spinner System developed by Headway Research, Inc.
    
Make sure you're wearing safety glasses when using the spinner! Glasses are on the wall to the right when you enter the room. Bring a micropipette and a small, lightweight piece of glass/plastic to spin on. The spinner uses a vacuum to keep the slide on the rotating bit, so no special attachment is necessary. But, if your slide that you're loading your  
 
Make sure you're wearing safety glasses when using the spinner! Glasses are on the wall to the right when you enter the room. Bring a micropipette and a small, lightweight piece of glass/plastic to spin on. The spinner uses a vacuum to keep the slide on the rotating bit, so no special attachment is necessary. But, if your slide that you're loading your  
Line 33: Line 35:     
P.S. For SSI Biology device: standard procedure for coating ETFE with fluoropel is 30s at 3000 RPM. Then cure on a hot plate: 80 degrees Celsius for 20 minutes, 150 degrees Celsius for 30 minutes.
 